Moscow University Chemistry Bulletin Vol. 46, No. 6, P. 378 (2005)
ChemNet
 
Previous article Next article Contents  

B. S. Lunin, S. N. Torbin

Formation of silica glass surface defects under heat treatment

Abstract

Some results of electronic microscope research of the surface of the resonators made from high and small internal stress silica glass are given. They show if there is internal stress in silica glass then the heat treatment leads to both decrease the stress and fast grow surface cracks with depth up to 0.5 mm. The grown of the surface defects leads to worsen optic and mechanical characteristics of the silica glass and to internal friction in the surface layer.
Moscow University Chemistry Bulletin.
2005, Vol. 46, No. 6, P. 378
   

Copyright (C) Chemistry Dept., Moscow State University, 2002
   Overview
   Editorial board
   Tables of Contents
   Subscription

The site is supported by Russian Foundation for Basic Research
  The using of published on this page materials is not allowed without special permission
Copyright (C) Chemisty Department of Moscow State University
Web-Editor: B.I.Pokrovskii
Web-design: Copyright (C) MIG and VVM
webmaster@www.chem.msu.su